CRNGO and CRNO Silicon Steel Coil/Plates Supplier
50W470 CRNGO Electrical Silicon Steel

50W470 silicon steel refers to a thickness of 0.5mm, non-oriented, and an iron loss value of 0.47 watts per kilogram. Baosteel electrical steel 50WW470 is a silicon steel widely used in the manufacture of energy-saving transformers and motors.

  • Type:CRNGO Silicon Steel

50W470 CRNGO Electrical Silicon Steel description

50W470 silicon steel refers to a thickness of 0.5mm, non-oriented, and an iron loss value of 0.47 watts per kilogram.

Baosteel electrical steel 50W470 is a silicon steel widely used in the manufacture of energy-saving transformers and motors. 50W470 CRNGO Silicon steel has excellent magnetic properties and is well suited for applications where low core loss and high magnetic permeability are critical.

One of the outstanding features of 50WW470 CRNGO Electrical Steel is its low core loss, which ensures minimal energy dissipation and helps improve overall efficiency. In addition, this steel has excellent thermal stability, allowing it to withstand high temperatures without affecting performance or structural integrity.

Silicon steel sheet is a soft magnetic alloy containing low carbon and silicon, with a silicon content of 0.5-4.5%. Adding silicon can increase the resistivity and maximum permeability of iron, reduce the coercivity, core loss (iron loss), and magnetic aging.

Mechanical Property
Grade Yeild Strength (N/mm2) Ultra-Tension Strength (N/mm2) Ductility(%) Hardness (HV1)
35W230 430 560 20.0 225
35W250 415 20.5550 20.5 215
35W270 400 515 20.5 215
35W300 360 480 21.5 195
35W360 350 480 23.5 190
35W440 275 420 27.5 165
35W550 265 415 33.5 160
50W250 430 560 19.0 230
50W270 410 550 21.5 225
50W290 395 545 22.5 220
50W310 385 510 24.5 210
50W350 350 475 26.5 190
50W400 320 460 36.0 170
50W470 295 425 35.0 160
50W600 280 410 37.0 140
50W800 285 405 38.5 135
50W1300(D) 250 360 40.0 115
Insulating Coating
Coating types M11 M21
Component Chromium containing , semi organic coating Chromium free, semi organic coating
Coating thickness(μm) 0.7~1.5 0.8~5.0
Interlayer resistance
(Ω•mm2 /slice)
≥100 ≥100
Adhesive property Class A or class B Class A or class B
Punching property Excellent Excellent
Antirust property Excellent Excellent
Heat resisting property Resistant annealing at 750 C, N2 protection, for 2h Annealing resistance in general